Influence of the molar ratio Sr:Bi:Ta in bismuth-strontium tantalum films SryBi2+xTa2O9 on structure and electrophysical properties

Capa

Citar

Texto integral

Acesso aberto Acesso aberto
Acesso é fechado Acesso está concedido
Acesso é fechado Somente assinantes

Resumo

Polycrystalline thin films of bismuth-strontium tantalum SryBi2+xTa2O9 with different molar ratio Sr:Bi:Ta were obtained by sol-gel method. The formation of a phase with a perovskite structure has been established. Phase transitions have been confirmed by dielectric spectroscopy. In the mode of polarization switching spectroscopy, remnant piezoelectric hysteresis loops were obtained, which confirms the ferroelectric nature of the synthesized SryBi2+xTa2O9 films.

Texto integral

Acesso é fechado

Sobre autores

D. Kiselev

Kotel’nikov Institute of Radio Engineering and Electronics (Fryazino Branch), Russian Academy of Sciences; National University of Science and Technology “MISIS”

Email: gvc@ms.ire.rssi.ru
Rússia, Fryazino, 141190; Moscow, 119049

E. Kurteva

National University of Science and Technology “MISIS”

Email: gvc@ms.ire.rssi.ru
Rússia, Moscow, 119049

A. Semchenko

F. Skorina Gomel State University

Email: gvc@ms.ire.rssi.ru
Belarus, Gomel, 246028

A. Boiko

Sukhoi State Technical University of Gomel

Email: gvc@ms.ire.rssi.ru
Belarus, Gomel, 246746

L. Sudnik

Powder Metallurgy Institute, Research Institute of Impulse Processes with Pilot Production

Email: gvc@ms.ire.rssi.ru
Rússia, Minsk, 220034

G. Chucheva

Kotel’nikov Institute of Radio Engineering and Electronics (Fryazino Branch), Russian Academy of Sciences

Autor responsável pela correspondência
Email: gvc@ms.ire.rssi.ru
Rússia, Fryazino, 141190

Bibliografia

  1. Muralt P., Polcawich R.G., Trolier-McKinstry S. // MRS Bulletin. 2009. V. 34. P. 658.
  2. Qiu Y., Gigliotti J.V., Wallace M. et al. // Sensors. 2015. V. 15. No. 4. P. 8020.
  3. Aabid A., Raheman M.A., Ibrahim Y.E. et al. // Sensors. 2021. V. 21. No. 2. P. 4145.
  4. Abdullaev D.A., Milovanov R.A., Volkov R.L. et al. // Russ. Technol. J. 2020. V. 8. No. 5. P. 44.
  5. Попов В.П., Антонов В.А., Тихоненко Ф.В. и др. // Изв. РАН. Сер. физ. 2023. Т. 87. № 6. С. 867; Popov V.P., Antonov V.A., Tikhonenko F.V. et al. // Bull. Russ. Acad. Sci. Phys. 2023. V. 87. No 6. P. 760.
  6. Li S., Wang Y., Yang M. et al. // Mater. Adv. 2022. V. 3. No. 14. P. 5735.
  7. Semchenko A.V., Ayvazyan G.Y., Malyutina-Bronskaya V.V. et. al. // Photonics. 2023. V. 10. P. 845.
  8. Semchenko A.V., Sidsky V.V. et. al. // Materials. 2021. V. 14. P. 1694.
  9. Bian J., Xue P., Zhu R. et al. // Appl. Mater. Today. 2020. V. 21. Art. No. 100789.
  10. Zanetti S.M., Bueno P.R., Leite E. et al. // J. Appl. Phys. 2001. V. 89. No. 6. P. 3416.

Arquivos suplementares

Arquivos suplementares
Ação
1. JATS XML
2. Fig. 1. X-ray diffraction patterns of SBT films with different Sr:Bi:Ta molar ratios: 1 — Sr(Bi3.4Ta2.8) O9; 2 — Sr0.4(Bi3.4Ta2.8) O9; 3 — Sr0.3(Bi3.5Ta2.8) O9.

Baixar (233KB)
3. Fig. 2. Temperature dependences of the permittivity at a frequency of 1 kHz (a) and field dependences of polarization (b) for SBT films obtained by the sol-gel method with different molar ratios of Sr:Bi:Ta: 1 — Sr(Bi3.4Ta2.8) O9; 2 — Sr0.4(Bi3.4Ta2.8) O9; 3 — Sr0.3(Bi3.5Ta2.8) O9.

Baixar (399KB)
4. Fig. 3. Topography (a, b, c) and surface potential signal (d, d, e) after preliminary polarization (dark square at –10 V, light square at +10 V) for films: a, d — Sr(Bi3.4Ta2.8)O9; b, d — Sr0.4(Bi3.4Ta2.8)O9; c, e — Sr0.3(Bi3.5Ta2.8)O9.

Baixar (1MB)
5. Fig. 4. Surface potential signal profiles (a) drawn in the middle of the images in Figure 3 (right column), images of piezoelectric hysteresis loops (b) for SBT films with different Sr:Bi:Ta molar ratios: 1 — Sr(Bi3.4Ta2.8)O9; 2 — Sr0.4(Bi3.4Ta2.8)O9; 3 — Sr0.3(Bi3.5Ta2.8)O9.

Baixar (285KB)

Declaração de direitos autorais © Russian Academy of Sciences, 2024